A Systematic Analysis of the Influence of Structure on Electrochemical Behavior Based on RDE and MEA Data for a Series of Commercial Pt/C Catalysts
Year: 2026
Type: article
Abstract: A systematic evaluation was carried out for the commercial Pt/C electrocatalyst series “PM” (Prometheus R&D LLC) with a platinum mass fraction from 5 to 70 wt.%. Materials with a Pt content of 5–40 wt.% were supported on Vulcan XC-72 carbon, while those with 50–70 wt.% were supported on a highly porous KetjenBlack EC-300J support. The composition, microstructure, electrochemically active surface area (ESA), oxygen reduction reaction (ORR) activity, and stability of the catalysts were studied using X-ray diffraction, TEM/HRTEM, TGA/DSC, cyclic voltammetry, CO-stripping, linear sweep voltammetry with a rotating disk electrode (RDE), and membrane electrode assembly (MEA) testing. It was shown that the average size of Pt nanoparticles (NPs) is 2.1–2.9 nm according to TEM data and 1.6–3.2 nm by XRD; it is controlled predominantly by the wet-synthesis stage rather than by the type of carbon support. With increasing Pt loading, a nonlinear decrease in ESA and mass activity in ORR is observed; the highest mass activity is demonstrated by PM20, while PM30-PM60 catalysts have similar values—328–394 A/g (Pt) and ESA up to 94 m2/g (Pt). The transition to KetjenBlack EC-300J support allows maintaining a uniform distribution of nanoparticles at high loadings and enhances the stability of the materials. The PM series catalysts are characterized by comparable or higher ESA and ORR mass activity than those of HiSPEC4000. In MEA tests, PM30-PM60 catalysts provide a maximum power density of up to 1000 mW/cm2 at a platinum utilization of 0.55–0.72. After durability testing, the loss of maximum power for materials on Vulcan XC-72 is 30–45%, whereas for PM50 and PM60 on KetjenBlack EC-300J it is 9–10%, with a residual power density of more than 2000 W/g(Pt) and more than 900 mW/cm2. It was established that the type of carbon support largely determines the stability of the catalysts, owing to differences in the degradation of both catalyst activity and the transport properties of the catalyst layers, as assessed by EIS. The obtained data can serve as reference data when comparing commercial and laboratory Pt/C catalysts for proton exchange membrane fuel cells (PEMFCs).
Source: Nanomaterials
DOI: 10.3390/nano16231544
Authors: Elizaveta Moguchikh(Investigation, Methodology, Visualization, Writing – original draft, Writing – review & editing), Angelina Pavlets(Investigation, Validation, Visualization, Writing – original draft), Kirill Paperzh(Formal analysis, Visualization, Writing – original draft), Alina Nevelskaya(Formal analysis, Investigation, Visualization), Yegor Beskopylny(Data curation, Methodology, Visualization, Writing – original draft), Dmitry Mauer(Formal analysis, Investigation), Ilya Kantsypa(Investigation, Validation), Yana Astravukh(Investigation, Validation), Alina Khudoley(Data curation, Investigation, Validation), Anna Gavrilova(Data curation, Validation), Ilya Pankov(Data curation, Investigation, Resources), Mikhail Tolstunov(Data curation, Investigation), Danil Alekseenko(Data curation, Formal analysis, Resources), Anastasia Alekseenko(Conceptualization, Funding acquisition, Project administration, Supervision, Writing – original draft, Writing – review & editing), Vladimir Guterman(Conceptualization, Supervision, Writing – review & editing), Sergey Belenov(Conceptualization, Formal analysis, Methodology, Project administration, Writing – original draft, Writing – review & editing)
Institutions: Southern Federal University, Southern Scientific Center
Language: English
Field: Energy
Domain: Physical Sciences
Open Access status: gold
Estimated APC paid: $2,896
OpenAlex ID: W7240054476