Abstract: The high activity of sulfated zirconia based catalysts for the isomerization of n-butane has lead to intensive study of these materials. Their skeletal isomerization ability is thought to arise from acidic sites on the catalyst, and attempts have been made to relate the acidity of sulfated zirconia to its activity, as has been successfully done for homogeneous catalysts and some classes of heterogeneous catalysts. However, the activity of sulfated zirconia is exceptional for its measured acidity. Promotion of sulfated zirconia through the addition of ~2 wt% of transition metal cations (manganese, iron) increases the low temperature isomerization activity by two orders of magnitude [1,2]. Despite the increased activity, the acidity of the promoted catalysts is no higher than that of sulfated zirconia [3]. The failure to explain activity through acidity has lead to the search for a second functionality in the catalyst, and suggestions for this additional functionality include oxidation/reduction reactions involving the promoter oxides [4]. We have reported a trend in the Mn oxidation state that was observed during activation and reaction of Mn-promoted sulfated zirconia (MnSZ) with n-butane, and was obtained from ex situ measurements [5]. Here we report results from in situ measurements of the Mn K edge during catalyst activation. In addition we present in situ and ex situ Zr K edge measurements which investigate the calcination step of the catalyst preparation. Data were reduced using the WinXAS software package [6].
Language: English
Subfield: Catalysis
Open Access status: green
OpenAlex ID: W782815875
FWCI:
Cites: 5
Cited by:
Related to: 10