Work

Processes for immobilization of high-level solid wastes by glass and ceramic matrices

Year: 1979
Type: conference-paper
Abstract: Processes for immobilization of waste SiC hulls and fissile particles from reprocessing of HTGR fuels are presented. Compressed cylinders of waste-matrix material were formed under approx. 35, 71, or 142 MPa and sintered at approx. 500 to 1025/sup 0/C for approx. 1 hour. The cylinders containing 50% SiC-25% soft glass-25% red clay possess the most desirable properties (high mechanical strength, low surface area and low leachability) of several different compositions studies. Within the pressure range studied, the pressure of cylinder formation does not appear to have any significant effect on those properties. 5 tables.
Language: English
Open Access status: green
OpenAlex ID: W96487609
FWCI:
Cites:
Cited by:
Related to: 10