Year: 1993
Type: article
Abstract: In the Al 2 O 3 -TiO 2 system, solid solutions of AIO(OH) gel are formed between 5 and 20 mol% TiO 2 by the simultaneous hydrolysis of aluminium and titanium alkoxides, followed by washing and drying. After dehydration γ-Al 2 O 3 solid solutions crystallize slowly from amorphous materials. At higher temperatures, rutile (TiO 2 ) is formed directly with the transformation of γ-Al 2 O 3 phases into corundum. Corundum-rutile composite ceramics with dispersed fine pores generated from the decomposition of Al 2 TiO 5 have been fabricated as follows:(1) hot pressing for 2 h at 1350°C under 35 MPa using γ-Al 2 O 3 solid solutions, (2) heating for 1 h at 1500°C to achieve the complete formation of Al 2 TiO 5 , and (3) annealing for 7 h at 1000°C to decompose of Al 2 TiO 5 into corundum and rutile. Their mechanical properties have been examined. The bending strength yields the maximum value of 365 MPa with 15 mol% TiO 2 content whereas the fracture toughness increases from 4.7 to 6.2 MPam 1/2 with increasing TiO 2 content.
DOI: 10.2497/jjspm.40.993
Institution: Doshisha University
Language: English
Subfield: Ceramics and Composites
Field: Materials Science
Domain: Physical Sciences
Open Access status: diamond
OpenAlex ID: W2313560456