Mössbauer Spectroscopic Study of Rust Formed on a Weathering Steel Exposed for 15 Years in an Industrial Environment

Year: 2000
Type: article
Abstract: The rust formed on weathering steel exposed to an industrial environment for 15 years was characterized by means of X-ray powder diffraction, Raman spectroscopy, electron probe microanalysis and Mössbauer spectroscopy. The rust consists of the crystalline α-FeOOH, γ-FeOOH and an X-ray amorphous phase. The amount of the X-ray amorphous phase exceeds 50% of the total amount of the rust. The 57Fe Mössbauer spectra observed at 10 K indicate that the rust contains only α-FeOOH and γ-FeOOH . The X-ray amorphous phase in the rust layer, which gives no peak in the X-ray diffraction pattern, is mainly α-FeOOH which shows a paramagnetic doublet due to the superparamagnetism occurring for small particle sizes at room temperature. The particle size of α-FeOOH is widely distributed and the inner rust layer contains relatively well-crystallized α-FeOOH compared to the outer layer.
Language: English
Open Access status: diamond
OpenAlex ID: W1963551243
FWCI: 1.326
Cites: 45
Cited by: 32
Related to: 10