Hot Isostatic Pressing of Composite Powder in the System ZrO2-WSi2. Part 2. Electrical and Mechanical Properties of ZrO2(2mol%Y2O3)/WSi2 Composites in the ZrO2 Rich Region and Their Laminated Materials.
Year: 1995
Type: article
Abstract: Well-densified composites with the compositions of ZrO2 (2Y) /WSi2=60/40 and 80/20mol% have been fabricated by hot isostatic pressing for 2 h at 1500°C and 196 MPa.Electric resistivities (ρ) between both composites change drastically; the former and latter composites correspond to the metallic and insulating materials, respectively. They are strongly dependent on the textures. Laminated materials with the compositions of ZrO2 (2Y) /WSi2=(60/40)/(80/20)/(60/40)mol% have been able to be prepared by the same technique. Overall electric resistivities in the perpendicular and parallel directions for the interfaces are determined to be ρ⊥≈1×1011 and ρ11≈1×10-4Ω·cm, respectively. The residual stress as much as≈200 MPa is induced in the interfaces.The fracture toughness (KIC) is much affected by the residual stress.
DOI: 10.5188/jsmerj.8.36
Institution: Doshisha University
Language: English
Subfield: Ceramics and Composites
Field: Materials Science
Domain: Physical Sciences
Open Access status: diamond
OpenAlex ID: W1978629028