Hydrolytic Degradation of Dental Composites
Year: 2014
Type: article
Abstract: This study evaluated the hydrolytic degradation of two experimental (C1, C2) and two commercial composite (Tetric EvoCeram and Premise) prepared to be used in dental restorations. Two experimental composites and two commercial composites were undergoing hydrolytic degradation in three different medium: distilled water, artificial saliva and alcoholic solution (50/50). The samples were investigated immediately after polymerisation with halogen lamp Optilux 501 and after 33 days of immersion in all three medium, using Fourier transforms infrared analysis (FTIR). FT-IR spectra of samples from the same composite immersed in distilled water, artificial saliva and alcoholic solution, revealed mostly reducing the intensity of the characteristic peaks of Si-O-Si bond less Tetric composite immersed in artificial saliva, which peak intensity remains unchanged.
Source: Key engineering materials
Language: English
Subfield: General Dentistry
Field: Dentistry
Domain: Health Sciences
Open Access status: hybrid
OpenAlex ID: W1995736331