Effect of Layer Thickness on I-V Characteristics of GaInP Nanofibers Fabricated by Electrospinning on n-Si Substrates
Year: 2017
Type: article
Abstract: GaInP nanofibers were formed on n-Si substrates by electrospinning method, using constant voltage (25 kV), height (6 cm), and flow rate (0.3 ml/h) during various process times (of 10, 20, 25 minutes).Characterization of the prepared samples was performed by X-ray diffraction, differential scanning calorimetry/thermal gravimetric analysis, scanning electron microscopy, and energy dispersive X-ray spectrometry.Furthermore, the currentvoltage measurements of the GaInP/n-Si samples have been carried out.The obtained results show that I -V characteristics of all GaInP/n-Si samples fabricated with three thicknesses of GaInP layers are rather in a good agreement with the theory and that they exhibit rectifying properties.
Source: Acta Physica Polonica A
Authors: N. Çiçek Bezir, A. Evcin, H. Okçu, R. Kayali, M. Kaleli, D.A. Aldemir
Language: English
Field: Materials Science
Domain: Physical Sciences
Open Access status: diamond
OpenAlex ID: W2761462226