Low temperature lithium/sulfur secondary battery. Annual progress report, December 1, 1974--December 1, 1975. [Ambient-temperature battery with dissolved S]
Year: 1976
Type: report
Abstract: The purpose of this program is to develop an ambient-temperature Li/S secondary battery. The proposed configuration is Li/organic electrolyte, dissolved S/catalytic electrode or current collector. This battery will have an energy density of 100 Wh/lb, including the weight of cell hardware. Investigations of S solubility and electrochemistry have been undertaken in polar, aprotic nonaqueous solvents, chosen for their stability toward Li. Highest S solubility was achieved if S was dissolved in the form of Li polysulfides, Li/sub 2/S/sub n/. Highest S solubilities were achieved in dimethyl sulfoxide (DMSO) and tetrahydrofuran (THF), where 9--10M S solutions were obtained as Li/sub 2/S/sub 9/-/sub 10/. The solutions of highest S concentrations were most readily prepared through the direct reaction of S/sub 8/ with Li/sub 2/S in the presence of the solvent. The discharge and charge capacities of such solutions, 1--2M in S, were measured galvanostatically between preset limits of 1 and 3.7V (vs. Li). Two plateaus were observed in DMSO, at 2.7V and at 2.2V. Discharge capacities of approximately 0.25 e/sup -//S were observed in THF and in methyl acetate. Recharge generally occurred between 2.5 and 3.0V. In DMSO, experiments showed that S/sub 8/ or S/sub 8//sup -2/ could not be reduced on C below S/sub 4//sup -2/, positive of 1.0V vs. Li/sup +//Li. However, S/sup -2/ and S/sub 4//sup -2/ could be readily oxidized on C up to S/sup -2//sub n greater than 10/, withoutthe formation of (insoluble) S/sub 8/. Only S/sub 8//sup -2/ gave S/sub 8/ precipitation upon oxidation. It was concluded that the cycling capacity of the dissolved Li/sub 2/S cathode was limited by the reduction of S/sup -2//sub n < 4/ on C. Other studies indicate that rechargeability of the negative will not be a special problem. 20 figures, 5 tables.
DOI: 10.2172/7123189
Authors: S Brummer, R Rauh, J Marston, F Shuker
Language: English
Subfield: Electrical and Electronic Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W301953449