Work

Adjusted Process Conditions in Laser Powder Bed Fusion to Obtain a Single-Crystal-Like Microstructure in IN718

Year: 2021
Type: article
Abstract: The nickel base alloy IN718 was manufactured by Laser Powder Bed Fusion (LPBF) using a laser spot size of 1024 μm and a laser power of 1.3 kW at a layer thickness of 160μm. The resulting porosity, microstructure and mechanical properties are presented. Very coarse and in build direction elongated grains are stacked to form a polycrystalline material with sharp single-crystal-like texture. The appearance of ∑5 grain boundaries between coincidence side lattices is recognized. Tensile testing shows highly anisotropic mechanical properties according to the revealed texture. Increasing the hatch distance reduces the severity of the texture.
Language: English
Open Access status: hybrid
OpenAlex ID: W3136560873
FWCI: 0.107
Cites: 13
Cited by: 2
Related to: 10