Work

Thermoelectric Property of Ball Milled Bi-Te-Sb Powder

Year: 2005
Type: article
Abstract: The p-type semiconductor $Bi_2Te_3-Sb_2Te_3$ thermoelectric materials were fabricated by melting, milling and sintering process and their thermoelectric properties were characterized. The compound materials were ball-milled with milling time and the powders were sintered by spark plasma sintering process. The ball milled powders had equiaxial shape and approedmately $1\~3{\mu}m$ in size. The figure of meritz of sintered thermoelectric materials decreased with milling time because of lowered electrical resistivity. The thermoelectric properties of $Bi_2Te_3-Sb_2Te_3$ materials have been discussed in terms of electrical property with ball mill process.