Multi-response optimization of sequential NaOH-KMnO4 treatment of sisal and banana fibers: Balancing tensile strength and water absorption with surface characteristics
Year: 2026
Type: article
Abstract: Natural fibres offer sustainable alternatives to synthetic reinforcements, but their hydrophilic and heterogeneous surfaces can promote water uptake and limit effective interaction with polymer matrices. Sequential chemical treatments can modify these characteristics; however, systematic multi-response optimization of NaOH-KMnO 4 treatment across different fibre types remains limited. This study optimized KMnO 4 concentration and treatment time following NaOH pretreatment of sisal and banana fibres using response surface methodology–central composite design (RSM-CCD), with tensile strength and water absorption as competing responses. Treatment-induced functional-group and morphological changes were evaluated using FTIR and SEM. All quadratic models were significant (p < 0.05), although their moderate R 2 values (0.712-0.764) indicated greater suitability for describing treatment–response trends than for high-precision prediction. Sisal tensile strength was significantly influenced by the concentration–time interaction, whereas its water absorption exhibited a significant quadratic dependence on KMnO 4 concentration. In contrast, both responses of banana fibres showed significant quadratic effects of treatment time, demonstrating fibre-specific treatment sensitivities. Multi-response optimization identified approximately 0.10% KMnO 4 and 4 min as favourable conditions for both fibres, predicting tensile strength/water absorption of 62.99 MPa/123% for sisal and 23 MPa/237% for banana. Experimental validation yielded 65.63 MPa/130.24% and 26.07 MPa/219.58%, respectively, corresponding to absolute percentage errors of 4.04-11.78%. FTIR indicated modification of non-cellulosic-associated functional groups, while SEM revealed increased surface roughness, fibrillation, etching, grooves and pits following sequential treatment. Overall, sisal exhibited the more favourable balance of tensile strength and water uptake. These findings demonstrate that sequential NaOH-KMnO 4 treatment requires fibre-specific optimization that balances competing responses rather than increasing treatment severity indiscriminately, providing a basis for subsequent evaluation of the treated fibres as polymer-composite reinforcements.
Source: Results in Materials
Institution: Busitema University
Language: English
Subfield: Polymers and Plastics
Field: Materials Science
Domain: Physical Sciences
Open Access status: gold
Estimated APC paid: $1,530
Funder: Busitema University
OpenAlex ID: W7204155995