Work

Dense alumina by combining ternary sintering additives with spark plasma sintering at 750°C

Year: 2026
Type: article
Abstract: Alumina ceramics possess excellent thermal, chemical, and mechanical properties but usually require sintering above 1600 °C, leading to high energy use and grain growth. Commercial alumina (95–96% purity) with conventional SiO 2 –MgO–CaO additives is also typically sintered at ≥1600 °C. In this study, a synergistic combination of a ternary oxide sintering aid (5 wt.% CuO–TiO 2 –Nb 2 O 5 ) and spark plasma sintering (SPS) was used to drastically lower the densification temperature of alumina. Fully dense alumina (≈100%) was achieved at 750 °C under 60 MPa and at 850 °C under 10 MPa, compared with pressureless sintering, which reached only 97% density at 1050 °C. SPS created a reductive environment that stabilised Cu + species and promoted liquid-phase-assisted densification while suppressing abnormal grain growth. In contrast, pressureless sintering led to CuO migration and niobium-rich secondary phases. SPS-processed samples showed finer, more uniform grains and comparable or higher hardness. Overall, combining ternary oxide additives with SPS enables energy-efficient, ultra-low-temperature densification of alumina with controlled microstructure.
Language: English
Open Access status: hybrid
Estimated APC paid: $3,830
OpenAlex ID: W7204998762
FWCI: 1.407
Cites: 89
Cited by: 1
Related to: 9