Abstract: Si using 80plus Reactive Ion Etcher (Graduate Student Fellow Program) Prepare by Prashanth Gopalan (4/3/2014) SiO2 etch • Ar = 38 sccm • CHF3 = 12 sccm • Pressure = 30 mTorr • Power = 200 W • T = 17.5 °C • Etching rate: 33 nm/min Note: Etch rate also depends on the sample size and percentage of the open area, which is not covered by resist film.Time and power dependence of etch depth (12/6/2013) Power dependence of etch rate (1/9/2014)