Work

Study of SeWaRe Failure in a Glass-Core Substrate with Redistribution Layers

Year: 2026
Type: conference-paper
Abstract: The demand for high-performance semiconductors continues to rise in the era of AI and glass substrates are emerging as a superior alternative to conventional substrates due to their thermal stability, smooth surface, high rigidity, large-area processability, better dielectric properties, etc. Mechanical dicing of large panel glass substrates leads to the near-mode I fracture failure commonly referred to as SeWaRe failure. SeWaRe ("splitting of the back" in Japanese) is the result of a cohesive crack originating at a singulated free edge that propagates through the bulk of the substrate. Existing literature has mostly focused on SeWaRe failure of glass substrates with thicknesses of less than or equal to 500 µm and consisting of less than or equal to double-sided 6 RDL layers. This study aims to examine SeWaRe failure in a 1000 µm-thick glass substrate consisting of single-sided 6 RDL layers. Experimental and simulated fracture behavior was obtained and reported in this study. Mechanical dicing of the test vehicle into individual coupons produced two main types of failure: (1) SeWaRe failure where a crack propagated through the bulk of the glass substrate near the dielectric-glass interface or (2) interfacial delamination between the copper and dielectric layers without any apparent SeWaRe failure. An innovative simulation approach that coupled the mechanics of the sequential fabrication process with the effects of multi-pass mechanical dicing was created to obtain the energy release rate for cracks of different sizes located at various distances below the dielectric and glass interface. The energy release rate exceeded the critical energy release rate only when the base of the defect was exposed and free edges were created.
Language: English
Open Access status: hybrid
OpenAlex ID: W7165045708
FWCI:
Cites: 12
Cited by:
Related to: 10